TAIRIPRO® T2502 Homopolymer PP Extrusion Grade
Tairipro T2502 is a premium homopolymer polypropylene resin in pellet form, engineered for extrusion and blow molding. It delivers high stiffness, excellent transparency, and superior heat resistance—ideal for creating lightweight, durable products. Trusted by industry leaders, Tairipro T2502 PP pellets ensure reliability and efficiency in high-performance manufacturing.
- Character: High stiffiness, Good transparency, Good heat resistance
- Application: Transparency pressure forming sheet,Portfolio, Bottles
Key technical data (ISO)
- Melt Flow Index: 1.8 g/10 min (230°C, 2.16 kg)
- Impact Strength: 59 kJ/m² (Notched, 23°C)
- Tensile Strength: 35 MPa
- Elongation at Break: >200%
- Molding Shrinkage: 1.5–1.9%
- Rockwell Hardness: R-100
Features & Benefits

Application

Related TAIRIPRO® PP Plastics
FCFC TAIRIPRO® T2502 PP Resin
FCFC TAIRIPRO® T1202 PP Resin
FCFC TAIRIPRO® T1002 PP Resin
FCFC TAIRIPRO® S1803 PP Resin
FCFC TAIRIPRO® S1005 PP Resin
FCFC TAIRIPRO® S1003 PP Resin
FCFC TAIRIPRO® S1040 PP Resin
FCFC TAIRIPRO® S1019 PP Resin
FCFC TAIRIPRO® K2051 PP Resin
FCFC TAIRIPRO® K1525 PP Resin
FCFC TAIRIPRO® K1108 PP Resin
FCFC TAIRIPRO® K1080 PP Resin
FCFC TAIRIPRO® K1023 PP Resin
FCFC TAIRIPRO® K1011AG PP Resin
FCFC TAIRIPRO® F2011 PP Resin
FCFC TAIRIPRO® F2003 PP Resin
FCFC TAIRIPRO® F1611 PP Resin
FCFC TAIRIPRO® B1101 PP Resin
FCFC Formosa TAIRIPRO® T4002
FCFC Formosa TAIRIPRO® T3002
FCFC Formosa TAIRIPRO® F4008
FCFC Formosa TAIRIPRO® F4007
FCFC Formosa TAIRIPRO® F4006
FCFC Formosa TAIRIPRO® K4750
FCFC Formosa TAIRIPRO® K4715
FCFC Formosa TAIRIPRO® K4650
FCFC Formosa TAIRIPRO® K4515
FCFC Formosa TAIRIPRO® K4038
FCFC Formosa TAIRIPRO® T8002
FCFC Formosa TAIRIPRO® B8001A3
Advanced Manufacturing